Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 340 g | 340 g | ASTM D1922 |
ExxonMobil Exact™ 4151 Ethylene-based Plastomer Resin Product Description: Exact 4151 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 4151 is designed for both monolayer and multilayer coe.. |
|||
Elmendorf Tear Strength TD | 340 g | 340 g | ASTM D1922 |
ExxonMobil LLDPE LL 1002.09 Linear Low Density Polyethylene Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |
|||
Elmendorf Tear Strength TD | 340 g | 340 g | ASTM D1922 |
ExxonMobil LLDPE LL 1002.80 Linear Low Density Polyethylene Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |
|||
Elmendorf Tear Strength TD | 340 g | 340 g | ASTM D1922 |
ExxonMobil LLDPE LL 1002X75 Linear Low Density Polyethylene Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |
|||
Elmendorf Tear Strength TD | 340 g | 340 g | gF; ASTM D1922 |
Braskem Green PE SLL218/21 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene Lower greenhouse gas emissions100% made from renewable raw materialsPerformance and Competitiveness: Green Polyethylene has the same characteristics as petrochemical polyethyleneApplications: Line.. |
|||
Elmendorf Tear Strength TD | 340 g | 340 g | gF; ASTM D1922 |
Braskem Green PE SLL318 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene Description: SLL118 is a Linear Low Density Polyethylene, copolymer of butene-1. Developed for blown film extrusion in blends with polyethylenes. Films obtained with this product show a good process.. |
|||
Elmendorf Tear Strength TD | 340 g | 340 g | gF; ASTM D1922 |
Braskem LL118 Blown Film Extrusion Linear Low Density Polyethylene Description: LL218/21 is a LLDPE Butene copolymer produced by Braskem. It was specially designed to provide outstanding processing performance. Films obtained with this grade show good physical and .. |
|||
Elmendorf Tear Strength TD | 340 g | 340 g | gF; ASTM D1922 |
Braskem LL218/21 Cast Film Extrusion Linear Low Density Polyethylene Liners, LDPE and HDPE blends; General use packages; Technical films for automatic packaging.Additives: Antiblock, DInformation provided by Braskem. |
|||
Elmendorf Tear Strength TD | 340 g | 340 g | ASTM-D1922 |
Braskem LL318 LLDPE Cast Film Extrusion Polyethylene Copolymer LL318 is a linear low-density polyethylene, copolymer of butene-1, produced by the Spherilene process. It was developed for cast film extrusion. Films obtained with this product show good mechanical.. |
|||
Elmendorf Tear Strength TD | 340 g | 340 g | ASTM-D1922 |
Braskem LL318 LLDPE Linear Low Density Extrusion Polyethylene LL318 is a linear low-density polyethylene, copolymer of butene-1, produced by the Spherilene process. It was developed for cast film extrusion. Films obtained with this product show good mechanical.. |