Polymer Property : Elmendorf Tear Strength TD = 420 g Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength TD 420 g
420 g
ASTM D1922
ExxonMobil Exceed™ 363C32 LDPE/Hexene Premium Cast Stretch Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 363C32 resin have outstanding tensile properties and..
Elmendorf Tear Strength TD 420 g
420 g
ASTM D1922
Iran Petrochemical (PCC) 12XF6 Linear Low Density Polyethylene
12XF6 is a high performance LLDPE (HP-LLDPE) blown film grade for high film strength applications.Information provided by Iran Petrochemical Commercial Co.
Elmendorf Tear Strength TD 420 g
420 g
ASTM D1922
Chevron Phillips MarFlex® D139 m-LLDPE Linear Low Density Polyethylene
Low Density PolyethyleneCustomer Benefits: Possesses the typical physical properties of metallocene polyethylenes with the added potential benefit of improved processability (bubble stability, down-..
Elmendorf Tear Strength TD 420 g
420 g
ASTM D1922
ExxonMobil Exceed™ 1518HA Metallocene Polyethylene Resin
Product Description: Exceed 1518HA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1518HA have outstanding tensile, impact strength and puncture. These superior strength propertie..
Elmendorf Tear Strength TD 420 g
420 g
ASTM D1922
ExxonMobil Exceed™ 2718CB Premium Cast Film Resin
Exceed 2718CB resin is a hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 2718CB resin have outstanding tensile properties and impact and puncture toughness..