Iran Petrochemical (PCC) 12XF6 Linear Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Blow Molding Grade , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) 12XF6 Linear Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
12XF6 is a high performance LLDPE (HP-LLDPE) blown film grade for high film strength applications.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.912 g/cc
0.0329 lb/in³
ASTM D1505
Melt Flow 0.60 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.60 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 11.5 MPa
1670 psi
ASTM D882
Film Tensile Strength at Yield, TD 11.2 MPa
1620 psi
ASTM D882
Film Elongation at Break, MD 600 %
600 %
ASTM D882
Film Elongation at Break, TD 760 %
760 %
ASTM D882
2% Secant Modulus 0.170 GPa
24.7 ksi
MD; ASTM D882
0.185 GPa
26.8 ksi
TD; ASTM D882
Elmendorf Tear Strength MD 220 g
220 g
ASTM D1922
Elmendorf Tear Strength TD 420 g
420 g
ASTM D1922
Dart Drop Test 175 g
0.386 lb
ASTM D1709
Film Tensile Strength at Break, MD 43.0 MPa
6240 psi
ASTM D882
Film Tensile Strength at Break, TD 35.0 MPa
5080 psi
ASTM D882
Optical Properties Metric English Comments
Haze 42 %
42 %
ASTM D1003
Gloss 35 %
35 %
ASTM D2457