Polymer Property : Dart Drop = 90.0 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 3.54 g/micron
90.0 g/mil
ASTM D1709
Huntsman Rexell® M3104 Blown Film Extrusion LLDPE  (discontinued **)
Linear-low medium density copolymer, cast film extrusion, FDA compliant.Features: Excellent combination of toughness, stiffness, and optics with good temperature resistance.Applications: Diaper film..
Dart Drop 3.54 g/micron
90.0 g/mil
ASTM D1709
ExxonMobil LD 051.LJ Shrink Film Resin  (discontinued **)
LD 051 blown film resins are designed for demanding heavy duty film applications, and combine excellent strength properties with outstanding processability. Used in heavy duty shipping bags and shr..
Dart Drop 3.54 g/micron
90.0 g/mil
ASTM D1709
ExxonMobil LD 051.LT Shrink Film Resin  (discontinued **)
LD 051 blown film resins are designed for demanding heavy duty film applications, and combine excellent strength properties with outstanding processability. Used in heavy duty shipping bags and shr..
Dart Drop 3.54 - 3.94 g/micron
90.0 - 100 g/mil
ASTM D1709
Huntsman PE 1008 Film Extrusion Polyethylene  (discontinued **)
Homopolymer, and FDA compliant.Features: Superior strength, good machinability, and heat seal characteristics.Applications: Film extrusion: industrial packaging, frozen food, produce bags, shrink, a..
Dart Drop 3.54 - 4.13 g/micron
90.0 - 105 g/mil
ASTM D1709
Huntsman PE 1011 Film Extrusion Polyethylene  (discontinued **)
Homopolymer, Drug Master File listed product, and FDA compliant.Features: Good impact strength, good machinability, heat seal and foaming characteristicsApplications: Film Extrusion: industrial line..
Dart Drop 3.54 g/micron
90.0 g/mil
ASTM D1709
Huntsman PE1031 Film Extrusion Polyethylene  (discontinued **)
Homopolymer, and FDA compliant.Features: Superior strength, good machinability, and heat seal characteristics.Applications: Film extrusion: clarity packaging, frozen food, produce bags, shrink, bund..
Dart Drop 3.54 g/micron
90.0 g/mil
ASTM D1709
Huntsman PE1033 Film Extrusion Polyethylene  (discontinued **)
Homopolymer, and FDA compliant.Features: Good opticals, impact strength, good processing properties, and stiffnessApplications: Film extrusion: general purpose packaging and film applications.FDA No..
Dart Drop 3.54 g/micron
90.0 g/mil
ASTM D1709
LyondellBasell Montell 16502F3 Butene LLDPE
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, no slip, no antiblockApplications: can liners and trash bags, blends, thin filmsMeets FDA..
Dart Drop 3.54 g/micron
90.0 g/mil
ASTM D1709
LyondellBasell Montell 16502F7 Butene LLDPE
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, low slip, medium antiblockApplications: can liners and trash bags, blends, thin filmsMeet..
Dart Drop 3.54 g/micron
90.0 g/mil
ASTM D1709
LyondellBasell Montell 16502F8 Butene LLDPE
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, medium slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMee..
Dart Drop 3.54 g/micron
90.0 g/mil
ASTM D1709
Westlake LF1050 Butene Linear Low Density Polyethylene
Westlake LF1050 is a butene LLDPE with high stiffness suitable for cast film extrusion. This material can be used at 100% or as blending stock with LDPE or MDPE.Application/UsesCast film extrusionPr..
Dart Drop 3.54 g/micron
90.0 g/mil
ASTM D1709
Westlake LF2040 Hexene Linear Low Density Polyethylene
Westlake LF2040 is a hexene LLDPE with excellent physical properties and heat sealing characteristics, which allow for down-gauging and blending with other materials. Typical applications include s..
Dart Drop 3.54 g/micron
90.0 g/mil
ASTM D1709
Total PPR Z9421 Polypropylene, Random Copolymer, Heat Sealable Film Grade
Color/Clarity/Impact. TOTAL Petrochemicals Polypropylene Z9421 is a low melting, high ethylene random copolymer with improved color, optics and impact properties.Heat Sealable. The very low melting..
Dart Drop 3.54 g/micron
90.0 g/mil
ASTM D1709
Formosa Plastics Formolene® L62030B Film (Hexene Grade) LLDPE
Hexene Copolymer (Barefoot)Applications: Cast stretch film and high quality packaging films requiring clarity and toughness.A Hexene Copolymer Linear Low Density Polyethylene for film applications i..
Dart Drop 3.54 g/micron
90.0 g/mil
ASTM D1709
ExxonMobil LL 3003.32 Cast Film Resin
Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p..
Dart Drop 3.54 g/micron
90.0 g/mil
ASTM D1709
ExxonMobil LL 3003.39 Cast Film Resin
Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p..
Dart Drop 3.54 g/micron
90.0 g/mil
ASTM D1709
Huntsman PE1158 EVA Film Extrusion  (discontinued **)
1.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: ..