Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Montell 16502F3 Butene LLDPE

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer LyondellBasell
Trade Name Montell
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF LyondellBasell Montell 16502F3 Butene LLDPE.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, no slip, no antiblockApplications: can liners and trash bags, blends, thin filmsMeets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications.Description: 16502 butene LLDPE film resin combine ease of processing with excellent optics and high film strength. These resins are well suited to replace LLDPE/LDPE blends in blown film applications. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirmnets of TSCA and DSL.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.916 g/cc
0.0331 lb/in³
ASTM D792
Thickness 25.4 microns
1.00 mil
Melt Flow 2.0 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
2.0 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 11.0 MPa
1600 psi
ASTM D882
Film Tensile Strength at Yield, TD 11.0 MPa
1600 psi
ASTM D882
Film Elongation at Break, MD 800 %
800 %
ASTM D882
Film Elongation at Break, TD 900 %
900 %
ASTM D882
Secant Modulus, MD 0.152 GPa
22.0 ksi
ASTM D882
Secant Modulus, TD 0.172 GPa
24.9 ksi
ASTM D882
Elmendorf Tear Strength MD 40 g
40 g
ASTM D1922A
Elmendorf Tear Strength TD 350 g
350 g
ASTM D1922A
Elmendorf Tear Strength, MD 1.57 g/micron
40.0 g/mil
ASTM D1922A
Elmendorf Tear Strength, TD 13.8 g/micron
350 g/mil
ASTM D1922A
Dart Drop 3.54 g/micron
90.0 g/mil
ASTM D1709
Dart Drop Test 90.0 g
0.198 lb
ASTM D1709A
Film Tensile Strength at Break, MD 37.9 MPa
5500 psi
ASTM D882
Film Tensile Strength at Break, TD 29.0 MPa
4210 psi
ASTM D882