Mechanical Properties Metric English Comments
Dart Drop 3.90 - 10.2 g/micron
99.1 - 260 g/mil
Average value: 7.35 g/micron Grade Count:3
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Film Grade". Each property range of values reported is minimum and m..