Mechanical Properties Metric English Comments
Dart Drop 3.90 g/micron
99.1 g/mil
F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709
Eastman 5251 LDPE 4% VA Copolymer, High Clarity, High Impact Film Resin for Laminations  (discontinued **)
Resin Type: VA CopolymerCharacteristics: Excellent adhesion, Excellent processability and bubble stability, High slip and antiblock, Good impact strengthApplications:Laminations, Heavy produce and s..
Dart Drop 3.90 g/micron
99.1 g/mil
F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709
Eastman 5254 LDPE 4% VA Copolymer, High Clarity, High Impact Film Resin for Laminations  (discontinued **)
Resin Type: VA CopolymerCharacteristics: Good adhesion, Good processability and bubble stability, Low slip, Medium antiblock, Good optical properties, Good impact strengthApplications:Laminations, H..
Dart Drop 3.90 g/micron
99.1 g/mil
F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709
Eastman 5272 LDPE 4% VA Copolymer, High Clarity, High Impact Film Resin  (discontinued **)
Resin Type: VA CopolymerCharacteristics: Good impact strength, Good bubble stability, Low coefficient of friction, Medium antiblock, Medium slip, Good low temperature properties, Good heat seal char..
Dart Drop 3.90 g/micron
99.1 g/mil
F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709
Eastman 5274 LDPE 4% VA Copolymer, High Clarity, High Impact Film Resin  (discontinued **)
Resin Type: VA CopolymerCharacteristics: Good impact strength, Good bubble stability, Low coefficient of friction, High antiblock, Medium slip, Good low temperature properties, Good heat seal charac..
Dart Drop 3.90 g/micron
99.1 g/mil
ASTM D1709
SCG Chemicals EL-Leneâ„¢ LD1902F Low Density Polyethylene Film
Key Characteristics:High strengthGood optical propertiesCan be blended with HDPE, LLDPESafe for food contactContains 1400 ppm slip content and 2400 ppm antiblocking contentRecommended Applications:G..
Dart Drop 3.90 g/micron
99.1 g/mil
ASTM D1709
SCG Chemicals EL-Leneâ„¢ LD1902FA Low Density Polyethylene Film
Key Characteristics:High strengthGood optical propertiesCan be blended with HDPE, LLDPESafe for food contactRecommended Applications:General purpose bag, big bagMedium-weight shrink filmInformation ..
Dart Drop 3.90 g/micron
99.1 g/mil
ASTM D1709B
DuPont Nucrel® 403 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
4 wt% Methacrylic Acid.Nucrel® 0403 is an ethylene-methacrylic acid copolymer resin available for use in blown and cast film extrusion and coextrusion equipment designed to process polyethylene res..
Dart Drop 3.90 g/micron
99.1 g/mil
Dow LDPE 133A Low Density Polyethylene, Blown Film Grade
DOW LDPE 133A resin is used for heavy duty blown film applications such as shrink film, shipping sacks, construction film, and other thick gauge film applications. It contains medium levels of antib..
Dart Drop 3.90 g/micron
99.1 g/mil
Dow LDPE 135A Low Density Polyethylene, Blown Film Grade
DOW LDPE 135A resin is used for heavy duty blown film applications such as shrink film, shipping sacks, construction film, and other thick gauge film applications. It contains medium levels of slip ..
Dart Drop 3.90 g/micron
99.1 g/mil
Dow LDPE 132I Low Density Polyethylene, Blown Film Grade
DOW LDPE 132I is a barefoot resin for heavy duty blown film applications such as shrink film, shipping sacks, construction film, and other thick gauge film applications. It complies with U.S. FDA re..
Dart Drop 3.90 - 10.2 g/micron
99.1 - 260 g/mil
Average value: 7.35 g/micron Grade Count:3
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Film Grade". Each property range of values reported is minimum and m..