Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 142 - 152 g/micron | 3610 - 3860 g/mil | Average value: 151 g/micron Grade Count:13 |
Overview of materials for Medium Density Polyethylene (MDPE), Rotational Molded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Rotational Molded". Each property range of values reported is minimu.. |