Mechanical Properties Metric English Comments
Dart Drop 142 - 152 g/micron
3610 - 3860 g/mil
Average value: 151 g/micron Grade Count:13
Overview of materials for Medium Density Polyethylene (MDPE), Rotational Molded
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Rotational Molded". Each property range of values reported is minimu..