Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 142 g/micron | 3610 g/mil | Instrumented Falling Weight (-4°F/-20°C); ASTM D3763 |
Borealis Borecene™ RM8343PL Linear Polyethylene for Rotational Molding Borecene RM8343PL is plasma treated linear medium density natural polyethylene for rotational molding with improved adhesion properties. The material is plasma treated to change the chemical struct.. |
|||
Dart Drop | 142 - 152 g/micron | 3610 - 3860 g/mil | Average value: 151 g/micron Grade Count:13 |
Overview of materials for Medium Density Polyethylene (MDPE), Rotational Molded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Rotational Molded". Each property range of values reported is minimu.. |