Polymer Property : Dart Drop = 2.36 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 2.36 g/micron
59.9 g/mil
ASTM D1709
Eastman 184MF Polyethylene Film  (discontinued **)
Polyethylene 184MF is a low-density formulation with medium slip and low antiblock. It is suggested for film applications where enhanced processability and high clarity are required. It is character..
Dart Drop 2.36 g/micron
59.9 g/mil
ASTM D1709A
Eastman E6838-923F Polyethylene  (discontinued **)
E6838-923F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require heat-sealing treated-to-treated film surfaces and where good clarit..
Dart Drop 2.36 g/micron
60.0 g/mil
ASTM D1709
ExxonMobil LD 135.09 Cast Packaging Film Resin  (discontinued **)
LD 135.09 is a homopolymer film resin with good clarity. It is suitable for processing in cast film equipment. Applications include food packaging, light to medium duty bags, and textile packaging..
Dart Drop 2.36 g/micron
60.0 g/mil
ASTM D1709
ExxonMobil LD 146.NH Cast Film Resin  (discontinued **)
LD 146.NH is a homopolymer film resin offering good clarity, toughness, and stiffness. It is used in food packaging and laminating film.Information provided by ExxonMobil Chemical
Dart Drop 2.36 g/micron
60.0 g/mil
ASTM D1709
ExxonMobil LD 146.NH Packaging Film Resin  (discontinued **)
LD 146.NH is a homopolymer film resin offering good clarity, toughness, and stiffness. It is used in food packaging and laminating film.Information provided by ExxonMobil Chemical
Dart Drop 2.36 g/micron
60.0 g/mil
F50; ASTM D1709
ExxonMobil Escorene® LD-103 LDPE Industrial Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer industrial film resin with excellent toughness. LD-103 has a low melt index which gives excellent impact strength and melt strength o..
Dart Drop 2.36 g/micron
60.0 g/mil
F50; ASTM D1709
ExxonMobil Escorene® LD-336 EVA Film Resin, Clarity, Very High Drawdown  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 3.5% vinyl acetate copolymer blown film resin capable of very high drawdown with excellent clarity.Applications: Very thin heat seal layers; Light..
Dart Drop 2.36 g/micron
60.0 g/mil
ASTM D1709
LyondellBasell Lupolex FA LLDPE
Description: Lupolex 25G FA is a linear low density polyethylene (LLDPE) used for blending, film, packaging, and bagsFeatures: AntioxidantGood Puncture ResistanceHigh RigidityHigh ClarityGood Heat S..
Dart Drop 2.36 g/micron
60.0 g/mil
ASTM D1709
LyondellBasell Purell® PE1840H Low Density Polyethylene, Blown Film, Injection Molding, Blow Fill & Seal, Extrusion Blow Molding
Purell PE 1840 H is a low density polyethylene with good flexibility and is delivered in pellet form. It is designed for small blow molding but can also be used in film applications and injection mo..
Dart Drop 2.36 g/micron
60.0 g/mil
ASTM D1709
Westlake Hifor Xtreme SC74849 Linear Low Density Polyethylene
WESTLAKE HIFOR Xtreme Polyethylene SC74849 is a high strength linear low density polyethylene designed for blown film extrusion. This resin contains no slip, no antiblock, and polymer processing aid..
Dart Drop 2.36 g/micron
60.0 g/mil
ASTM D1709
ExxonMobil LL 1107x93 Blown Film Resin
Product Description: LL 1107 resins are fractional melt index butane LLDPE blown film resins. Films made with LL 1107 resins have good stiffness and tensile strength. Theses resins’ strength and dr..
Dart Drop 2.36 g/micron
60.0 g/mil
ASTM D1709
ExxonMobil LL 1107x95 Blown Film Resin
Product Description: LL 1107 resins are fractional melt index butane LLDPE blown film resins. Films made with LL 1107 resins have good stiffness and tensile strength. Theses resins’ strength and dr..
Dart Drop 2.36 - 30.0 g/micron
59.9 - 762 g/mil
Average value: 6.06 g/micron Grade Count:12
Overview of materials for Low Density Polyethylene (LDPE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum ..