Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus | 83.0 MPa | 12000 psi | ASTM D790 |
LG Chemical LC100 Polyolefin Elastomer Features: Excellent toughness with flexible performance, High clarity and low temperature sealability. High performance in footwear applicationApplication: Polymer modification, Shoe sole, Film coex.. |