Polymer Property : 1% Secant Modulus = 83.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus 83.0 MPa
12000 psi
ASTM D790
LG Chemical LC100 Polyolefin Elastomer
Features: Excellent toughness with flexible performance, High clarity and low temperature sealability. High performance in footwear applicationApplication: Polymer modification, Shoe sole, Film coex..