Polymer Property : Shear Strength = 11.53 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 11.53 MPa
1672 psi
Lap
Epoxy Technology EPO-TEK® H20-LC Electrically Conductive, Silver Epoxy
Product Description: EPO TEK® H20E-LC is a two component, silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is also used exte..
Shear Strength 11.53 MPa
1672 psi
Lap
Epoxy Technology EPO-TEK® H55 Epoxy
Material Description: A two component, thixotropic and high temperature epoxy designed to be used for hybrids and PCB applications.Information Provided by Epoxy Technology