Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 11.53 MPa | 1672 psi | Lap |
Epoxy Technology EPO-TEK® H20-LC Electrically Conductive, Silver Epoxy Product Description: EPO TEK® H20E-LC is a two component, silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is also used exte.. |
|||
Shear Strength | 11.53 MPa | 1672 psi | Lap |
Epoxy Technology EPO-TEK® H55 Epoxy Material Description: A two component, thixotropic and high temperature epoxy designed to be used for hybrids and PCB applications.Information Provided by Epoxy Technology |