Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Shear Strength = 131 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 131 MPa

@Thickness 1.57 mm
19000 psi

@Thickness 0.0620 in
Perpendicular
Industrial Laminates/Norplex NP841 Glass Fabric  (discontinued **)
Description: Woven glass fabric with phenolic resin. Contains Kocite® for controlled conductivity. Acts as static electricity drain to protect electrical and electronic equipment.Thickness Tested: ..