Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 131 MPa @Thickness 1.57 mm |
19000 psi @Thickness 0.0620 in |
Perpendicular |
Industrial Laminates/Norplex NP841 Glass Fabric
(discontinued **) Description: Woven glass fabric with phenolic resin. Contains Kocite® for controlled conductivity. Acts as static electricity drain to protect electrical and electronic equipment.Thickness Tested: .. |