Material Notes:
Description: Woven glass fabric with phenolic resin. Contains Kocite® for controlled conductivity. Acts as static electricity drain to protect electrical and electronic equipment.Thickness Tested: 0.062", 0.125" & 0.500"
Physical Properties Metric English Comments
Specific Gravity 1.85 g/cc
1.85 g/cc
Moisture Absorption at Equilibrium 0.40 %

@Thickness 1.57 mm
0.40 %

@Thickness 0.0620 in
Mechanical Properties Metric English Comments
Hardness, Rockwell M 100 - 120

@Thickness 1.57 mm
100 - 120

@Thickness 0.0620 in
Tensile Strength, Yield 234 MPa

@Thickness 3.17 mm
34000 psi

@Thickness 0.125 in
CW
290 MPa

@Thickness 3.17 mm
42000 psi

@Thickness 0.125 in
LW
Flexural Strength 276 MPa

@Thickness 1.57 mm
40000 psi

@Thickness 0.0620 in
CW
345 MPa

@Thickness 1.57 mm
50000 psi

@Thickness 0.0620 in
LW
Flexural Modulus 9.65 GPa

@Thickness 1.57 mm
1400 ksi

@Thickness 0.0620 in
CW
11.0 GPa

@Thickness 1.57 mm
1600 ksi

@Thickness 0.0620 in
LW
Compressive Strength 414 MPa

@Thickness 12.7 mm
60000 psi

@Thickness 0.500 in
Flatwise
Shear Strength 131 MPa

@Thickness 1.57 mm
19000 psi

@Thickness 0.0620 in
Perpendicular
Izod Impact, Unnotched 4.27 J/cm

@Thickness 12.7 mm
8.00 ft-lb/in

@Thickness 0.500 in
CW, E-48/50
5.87 J/cm

@Thickness 12.7 mm
11.0 ft-lb/in

@Thickness 0.500 in
LW, E-48/50
Thermal Properties Metric English Comments
CTE, linear 15.0 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
8.33 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis
CTE, linear, Transverse to Flow 18.0 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
10.0 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis
Maximum Service Temperature, Air 175 °C
347 °F
Maximum Operating Temperature
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Surface Resistivity per Square 10000 - 20000 ohm

@Thickness 1.57 mm
10000 - 20000 ohm

@Thickness 0.0620 in
Condition A
Descriptive Properties Value Comments
Bond Strength 1,600 lb