Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 10.3 - 12.4 MPa | 1500 - 1800 psi | |
ITW Plexus Plexusâ„¢ MA422 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive, medium open time.Information provided by Illinois Tool Works. |
|||
Shear Strength | 10.3 - 12.4 MPa | 1500 - 1800 psi | |
ITW Plexus Plexusâ„¢ MA425 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive, long open time.Information provided by Illinois Tool Works. |
|||
Shear Strength | 8.96 - 12.4 MPa | 1300 - 1800 psi | |
ITW Plexus Plexusâ„¢ MA550 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Excellent marine adhesive, UV stable.Information provided by Illinois Tool Works. |