Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Shear Strength = 24.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 24.8 MPa
3600 psi
In-Plane S12; ASTM D5379
Polystrand ThermoPro™ IE6010 Unitape Unidirectional Polypropylene-Glass Composite
Fiber Orientation is 0°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary thermoplastic polymer ..
Shear Strength 24.8 MPa

@Temperature 23.0 °C
3600 psi

@Temperature 73.4 °F
Hexcel® HexPly® F515 Epoxy Resin, 7781 Glass Fabric
Hexcel designation: 7781-38"-F515; Fiber 75-1/0Information provided by HexCel
Shear Strength 24.8 MPa
3600 psi
CRS Overlap, Hydraulic Oil at RT
3M Scotch-Weld™ 183 B/A Tan Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir..
Shear Strength 24.8 MPa
3600 psi
Overlap, CRS MEK/abrade/MEK
3M Scotch-Weld™ DP460 NS Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..
Shear Strength 24.8 MPa
3600 psi
Overlap, CRS, Cohesive Failure
3M Scotch-Weld™ DP810 Black Structural Adhesive
3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre..
Shear Strength 24.8 MPa

@Temperature 24.0 °C
3600 psi

@Temperature 75.2 °F
Overlap
3M Scotch-Weld™ DP810 Black Structural Adhesive
3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre..
Shear Strength 24.8 MPa
3600 psi
Overlap, Etched Aluminum, 5% Salt solution for 14 days, Cohesive Failure
3M Scotch-Weld™ DP920 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i..
Shear Strength 24.8 MPa

@Temperature 24.0 °C
3600 psi

@Temperature 75.2 °F
Overlap
3M Scotch-Weld™ DP810 Tan Structural Adhesive
3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre..
Shear Strength 24.8 MPa
3600 psi
Overlap, Al-MEK/Abrade/MEK, Cohesive Failure
3M Scotch-Weld™ LSB60 Toughened Epoxy Adhesives
3M™ Scotch-Weld™ Toughened Epoxy Adhesive LBS60 is a high performance, two-part, toughened epoxy adhesives offering outstanding shear adhesion and very high levels of durability with a choice of f..
Shear Strength 24.8 MPa
3600 psi
Lap, Alum to Alum
Atom Adhesives AA-BOND F131 Epoxy Adhesive
AA-BOND F131 is two parts fiber-optic adhesive used for terminating ALL types of fiber-optic connectors as well as LED displays, lenses and other optical components. AA-BOND F131 produces a typical ..
Shear Strength >= 24.8 MPa
>= 3600 psi
Tensile, Al to Al
Master Bond Supreme 10HTND-3 Non-Drip Epoxy Resists High Temperatures
Description: Master Bond Supreme 10HTND-3 features a blend of performance properties including both high shear and peel strengths along with a totally non-drip application feature. This one componen..