Atom Adhesives AA-BOND F131 Epoxy Adhesive

Category Polymer , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Atom Adhesives
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Atom Adhesives AA-BOND F131 Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AA-BOND F131 is two parts fiber-optic adhesive used for terminating ALL types of fiber-optic connectors as well as LED displays, lenses and other optical components. AA-BOND F131 produces a typical Tg of 95 °C thus meeting specification requirements of connector’s manufacturers. AA-BOND F131 is two part, low viscosity system can be cured at room temperature or as fast as 15 minutes at 90 °C.Appearance: Clear Cure Type: Heat cure or Room TemperatureBenefits:Low viscosity Mix Ratio by weight: 100:30/Resin:Hardener Typical Application: ALL types of fiber-optic connectors as well as LED displays, lenses and other optical components.Information provided by Atom Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
uncured
Viscosity 1600 - 2000 cP
1600 - 2000 cP
uncured
Mechanical Properties Metric English Comments
Hardness, Shore D 77
77
Shear Strength 24.8 MPa
3600 psi
Lap, Alum to Alum
Izod Impact, Notched 0.117 J/cm
0.220 ft-lb/in
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Glass Transition Temp, Tg 95.0 °C
203 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 90.0 °C
0.250 hour

@Temperature 194 °F
1 drop applications
60.0 min

@Temperature 65.0 °C
1.00 hour

@Temperature 149 °F
1080 min

@Temperature 25.0 °C
18.0 hour

@Temperature 77.0 °F
Shelf Life 12.0 Month
12.0 Month
uncured
Descriptive Properties Value Comments
Thixotropic Index 1