Polymer Property : Shear Strength = 2400 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 16.5 MPa
2400 psi
Indium Corp. Indalloy 242 Tin-Lead Solder Alloy
Information Provided by Indium Corporation
Shear Strength >= 16.5 MPa
>= 2400 psi
Lap, Al/Al
Master Bond EP38 Low Viscosity, Fast Curing, Two Component Epoxy
Master Bond Polymer System EP38 is a fast curing, low viscosity, optically clear two component epoxy system for high performance coating, bonding and sealing. EP38 has a unique balance of favorable ..
Shear Strength >= 16.5 MPa
>= 2400 psi
Master Bond EP45HTMED Epoxy Resists Radiation and Steam Sterilization
Description: Master Bond Polymer System EP45HTMED is a two component heat cured epoxy system for high performance structural bonding, sealing, coating and casting. It is especially designed for the ..
Shear Strength 16.5 MPa

@Temperature 24.0 °C
2400 psi

@Temperature 75.2 °F
Overlap, Steel Solvent Wipe; ASTM D1002-72
3M Scotch-Weld™ 1751 B/A Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 1751 B/A is a gray, aluminum filled, two-part, room temperature curing structural adhesive.Information provided by 3M
Shear Strength 16.5 - 17.2 MPa
2400 - 2500 psi
CRS Overlap
3M Scotch-Weld™ 183 B/A Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flowable product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent e..
Shear Strength 16.5 MPa
2400 psi
Overlap, Aluminum; ASTM D1002-64
3M Scotch-Weld™ CA9 Instant Adhesive
3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Slower setting version of CA8 for wire tacking and coil terminating. Meets CID A-A-3097, Type II, C..
Shear Strength 16.5 MPa
2400 psi
Overlap, Stainless Steel MEK/abrade/MEK
3M Scotch-Weld™ DP460 NS Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..
Shear Strength 16.5 MPa

@Temperature 24.0 °C
2400 psi

@Temperature 75.2 °F
Overlap
3M Scotch-Weld™ DP8005 Black Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl..
Shear Strength 16.5 MPa

@Temperature 24.0 °C
2400 psi

@Temperature 75.2 °F
Overlap
3M Scotch-Weld™ DP8010NS Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010NS is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polyprop..
Shear Strength 16.5 MPa
2400 psi
Overlap, CRS - with Ferrocote 6130 Draw Lube, Cohesive failure/Adhesive Failure; ASTM D1002
3M Scotch-Weld™ DP920 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i..
Shear Strength 16.5 MPa
2400 psi
ASTM D1002-94
Aremco Aremco-Bond™ 2200 High Performance Epoxide
Glass Fiber- and Kevlar-Reinforced, Epoxy-Novolac; High Strength, Excellent Abrasion and Corrosion Resistance
Shear Strength 16.5 MPa
2400 psi
Overlap, Oak, Substrate/Cohesive Failure
3M Scotch-Weld™ Thick Instant Wood Adhesives and Surface Activator
3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t..
Shear Strength 16.5 MPa
2400 psi
Overlap, Aluminum; ASTM D1002-64
3M Scotch-Weld™ CA7 Instant Adhesive
3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Very fast setting and excellent adhesion to metals, plastics, and rubbers.Information provided by 3..
Shear Strength 16.5 MPa

@Temperature 24.0 °C
2400 psi

@Temperature 75.2 °F
Overlap
3M Scotch-Weld™ DP8005 Translucent Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl..
Shear Strength 16.5 MPa
2400 psi
Overlap, Cold Rolled Steel (oily)
3M Scotch-Weld™ DP820 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP820 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability ..
Shear Strength 16.5 MPa
2400 psi
Lap, Alum to Alum
Atom Adhesives AA-BOND 2170 Epoxy Adhesive
AA-BOND 2170 is a flexible thixotropic bonding adhesive designed for bonding all types of plastics including nylon, PVC, polyethylene, acrylic, lexan, kapton or almost any thermoplastic substrate. A..
Shear Strength 16.5 MPa

@Temperature 24.0 °C
2400 psi

@Temperature 75.2 °F
Aluminum Overlap; ASTM D1002
3M Scotch-Weld™ 3501 B/A Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 3501 B/A Gray is a rapid room temperature curing, two-part epoxy adhesives for use in bonding many metals, wood, and a variety of plastics. Equal parts by volume ar..
Shear Strength 16.5 MPa

@Temperature 24.0 °C
2400 psi

@Temperature 75.2 °F
Aluminum Overlap; ASTM D1002
3M Scotch-Weld™ DP 3501 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP 3501 is a rapid room temperature curing, two-part epoxy adhesives for use in bonding many metals, wood, and a variety of plastics. Equal parts by volume are easi..