Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 22.1 MPa | 3200 psi | Bond, Al to Al, RT Cure |
Master Bond EP30P Epoxy Bonds Glass, Polycarbonates and Acrylics Description: Master Bond Polymer Adhesive EP30P is a two component, transparent, low viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulating and casting. It is for.. |
|||
Shear Strength | >= 22.1 MPa | >= 3200 psi | Bond, Al to Al |
Master Bond EP30LV Optically Clear, Low Viscosity Epoxy Adhesive Description: Master Bond Polymer System EP30LV is a low viscosity, two component epoxy adhesive for general purpose bonding, coating, sealing and casting formulated to cure at room temperature or mo.. |
|||
Shear Strength | >= 22.1 MPa | >= 3200 psi | Bond, Al to Al |
Master Bond Supreme 11AOHTLO Epoxy Passes NASA Low Outgassing Tests Description: Master Bond Supreme 11AOHTLO is a two component epoxy resin system for high performance bonding and sealing. Although, it is formulated to cure at room temperature, the best cure schedu.. |
|||
Shear Strength | 22.1 MPa | 3200 psi | Overlap, Aluminum Oakite degrease |
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat.. |
|||
Shear Strength | 22.1 MPa | 3200 psi | Overlap at 2 hrs after bonding |
3M Scotch-Weld™ DP810 Black Structural Adhesive 3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre.. |
|||
Shear Strength | 22.1 MPa | 3200 psi | Overlap, CRS-MEK/Abrade/MEK, Cohesive/Adhesive Failure |
3M Scotch-Weld™ LSB60 Toughened Epoxy Adhesives 3M™ Scotch-Weld™ Toughened Epoxy Adhesive LBS60 is a high performance, two-part, toughened epoxy adhesives offering outstanding shear adhesion and very high levels of durability with a choice of f.. |
|||
Shear Strength | 22.1 MPa @Temperature 24.0 °C |
3200 psi @Temperature 75.2 °F |
Overlap, Etched Aluminum; ASTM D1002 |
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |