Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Shear Strength = 45.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 45.0 MPa
6530 psi
In-Plane
Hexcel® HexPly® 954-3A Curing Cyanate Resin, M60J Fiber
Information provided by HexCel
Shear Strength 45.0 MPa
6530 psi
In-Line; ASTM D5379
Hexcel® HexMC® C/2000/R1A Carbon Epoxy Molding Composite
HexMC® is a high performance carbon molding composite, specifically designed for compression molding. The epoxy matrix and high carbon fiber volume content enable components to be molded for a wide..
Shear Strength 45.0 MPa
6530 psi
I.L.S.S. short beam shear per ASTM D5379
Hexcel® HexMC™ C / 2000 / R1 Composite SMC
High performance sheet-molding compound, specifically designed for compression molding. The epoxy matrix and high carbon fiber volume enable components to be molded for a wide range of applications..
Shear Strength 45.0 MPa

@Temperature 100 °C
6530 psi

@Temperature 212 °F
0º, ILSS (Short Beam), Wet; EN2563
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, TVR380/26% Fiber
Information provided by HexCel
Shear Strength 45.0 MPa

@Temperature 100 °C
6530 psi

@Temperature 212 °F
In-Plane, Wet; EN6031
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, TVR380/26% Fiber
Information provided by HexCel
Shear Strength >= 45.0 MPa
>= 6530 psi
Parallel to laminations; IEC 1212-2 5.6
Hippe MF CC 201 Woven Cotton Cloth Reinforced Melamine Resin - Sheet
Used in mechanical and electrical applications (coarse weave: >130 g/m2, =30 threads/cm). Arc and tracking resistant.Information provided by Hippe.
Shear Strength 45.0 MPa

@Temperature 80.0 °C
6530 psi

@Temperature 176 °F
Warp ILSS
Hexcel® HexPly® M26/M26T 120°C (250°F) Curing Epoxy Matrix, M26/45%/G1070 Carbon Fabric
6K T300J 370 gsmInformation provided by HexCel