Mechanical Properties Metric English Comments
Shear Strength 63.4 MPa

@Temperature 23.9 °C
9200 psi

@Temperature 75.0 °F
Short-Beam, Dry; Oven Cure 250°F, 90 min; ASTM D2344
Park Electrochemical Nelcote® E-763 Epoxy Prepreg, 3K PW Carbon Reinforced
Nelcote® E-763 is a modified epoxy system with a nominal 250°F cure temperature. E-763 provides a transparent resin surface on the finished part which gives finished part surfaces a cosmetic attra..
Shear Strength 63.4 MPa

@Temperature 23.9 °C
9200 psi

@Temperature 75.0 °F
Short Beam; Dry; ASTM D2344
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 4503 Quartz Reinforced
Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp..
Shear Strength 63.4 MPa
9200 psi
ASTM D732
Quadrant EPP Quadrant 1000 LSP PC Extruded Unfilled Polycarbonate
Shear Strength 63.4 MPa
9200 psi
ASTM D732
Quadrant EPP Quadrant PC 1000 Extruded, Unfilled, Polycarbonate (ASTM Product Data Sheet)
Shear Strength 63.4 MPa
9200 psi
Average value: 63.4 MPa Grade Count:3
Overview of materials for Polycarbonate, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp..
Shear Strength 63.4 MPa

@Temperature 24.0 °C
9200 psi

@Temperature 75.2 °F
Short Beam, Dry
Hexcel® HexPly® F522 Epoxy Resin, F3C584 Carbon Fabric
Hexcel designation: F3C584-42"-F522; Fiber: Toho® G30/500-3KInformation provided by HexCel
Shear Strength 63.4 MPa
9200 psi
uncured
Atom Adhesives AA-DUCT 2979 Epoxy Adhesive
AA-DUCT 2979 is a fast curing one part epoxy adhesive with superior electrical conductivity and bonding capability. AA-DUCT 2979 has been shown to retain their properties through hundreds of hours o..
Shear Strength 63.4 MPa
9200 psi
ASTM D732
Quadrant EPP Quadrant LSG PC (ASTM Product Data Sheet)