Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 63.4 MPa @Temperature 23.9 °C |
9200 psi @Temperature 75.0 °F |
Short-Beam, Dry; Oven Cure 250°F, 90 min; ASTM D2344 |
Park Electrochemical Nelcote® E-763 Epoxy Prepreg, 3K PW Carbon Reinforced Nelcote® E-763 is a modified epoxy system with a nominal 250°F cure temperature. E-763 provides a transparent resin surface on the finished part which gives finished part surfaces a cosmetic attra.. |
|||
Shear Strength | 63.4 MPa @Temperature 23.9 °C |
9200 psi @Temperature 75.0 °F |
Short Beam; Dry; ASTM D2344 |
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 4503 Quartz Reinforced Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp.. |
|||
Shear Strength | 63.4 MPa | 9200 psi | ASTM D732 |
Quadrant EPP Quadrant 1000 LSP PC Extruded Unfilled Polycarbonate |
|||
Shear Strength | 63.4 MPa | 9200 psi | ASTM D732 |
Quadrant EPP Quadrant PC 1000 Extruded, Unfilled, Polycarbonate (ASTM Product Data Sheet) |
|||
Shear Strength | 63.4 MPa | 9200 psi | Average value: 63.4 MPa Grade Count:3 |
Overview of materials for Polycarbonate, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Shear Strength | 63.4 MPa @Temperature 24.0 °C |
9200 psi @Temperature 75.2 °F |
Short Beam, Dry |
Hexcel® HexPly® F522 Epoxy Resin, F3C584 Carbon Fabric Hexcel designation: F3C584-42"-F522; Fiber: Toho® G30/500-3KInformation provided by HexCel |
|||
Shear Strength | 63.4 MPa | 9200 psi | uncured |
Atom Adhesives AA-DUCT 2979 Epoxy Adhesive AA-DUCT 2979 is a fast curing one part epoxy adhesive with superior electrical conductivity and bonding capability. AA-DUCT 2979 has been shown to retain their properties through hundreds of hours o.. |
|||
Shear Strength | 63.4 MPa | 9200 psi | ASTM D732 |
Quadrant EPP Quadrant LSG PC (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic Products. |