Material Notes:
AA-DUCT 2979 is a fast curing one part epoxy adhesive with superior electrical conductivity and bonding capability. AA-DUCT 2979 has been shown to retain their properties through hundreds of hours of rapid temperature cycling and has also high impact absorption and stress resistance. These qualities make it an excellent choice for a number of electronic applications especially in "under the hood" and other harsh operating environments. AA-DUCT 2979 has a shelf life of at least 6 months when stored at -40°C. It contains no volatile, harmful solvents or lead, and conforms to all of the requirements of the solder replacement market.Appearance: SilverCure Type: Heat cureMix Ratio by weight: 100:5/Resin:Hardener Benefits: High strengthExcellent mechanical, electrical properties Substrates: Excellent choice for Integrated Circuits, aluminum, copper, magnesium, steel, bronze, nickel, ceramic, glass, phenolic and G-10 epoxy glass boards. Typical Application: Applications where high impact absorption and stress resistance is requiredInformation provided by Atom Adhesives
Physical Properties Metric English Comments
Specific Gravity 3.50 g/cc
3.50 g/cc
uncured
Viscosity 65000 cP
65000 cP
uncured
Mechanical Properties Metric English Comments
Hardness, Shore D 86
86
cured
Shear Strength 63.4 MPa
9200 psi
uncured
Adhesive Bond Strength 12.1 MPa
1750 psi
uncured
Thermal Properties Metric English Comments
CTE, linear 57.0 µm/m-°C
31.7 µin/in-°F
uncured
Thermal Conductivity 0.901 W/m-K
6.25 BTU-in/hr-ft²-°F
uncured
Maximum Service Temperature, Air 175 °C
347 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Glass Transition Temp, Tg 45.0 °C
113 °F
Electrical Properties Metric English Comments
Volume Resistivity 0.00030 ohm-cm
0.00030 ohm-cm
cured
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 150 °C
0.167 hour

@Temperature 302 °F
60.0 min

@Temperature 125 °C
1.00 hour

@Temperature 257 °F
Pot Life 259200 min
259200 min
Shelf Life 6.00 Month
6.00 Month
uncured
Descriptive Properties Value Comments
Thixotropic Index 3.4