Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 72.0 - 90.0 MPa | 10400 - 13100 psi | Average value: 81.0 MPa Grade Count:8 |
Overview of materials for Nylon 66, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |
|||
Shear Strength | 72.0 MPa @Temperature 22.0 °C |
10400 psi @Temperature 71.6 °F |
0° |
Hexcel® HexPly® 954-3 Curing Cyanate Resin, G80-600 Fiber Information provided by HexCel |
|||
Shear Strength | 72.0 MPa | 10400 psi | ASTM D732 |
Cast Nylons Nycast® 6MPB Plasticized Nylon 6 A plasticized Type 6 material, NYCAST® 6MPB is formulated for use as pile driver caps or cushion pads. Data provided by the manufacturer, Cast Nylons Limited.The data below are average values prese.. |
|||
Shear Strength | 72.0 MPa | 10400 psi | ASTM D732 |
Cast Nylons Nycast® 6MPY Plasticized Nylon 6 A plasticized Type 6 material, NYCAST® 6MPY is formulated for use as pile driver caps or cushion pads. Data provided by the manufacturer, Cast Nylons Limited.The data below are average values prese.. |
|||
Shear Strength | 72.0 MPa | 10400 psi | ASTM D732 |
Cast Nylons Nycast® 6PA-Blue Nylon 6 NYCAST® 6 PA-Blue along with NYCAST® 6 PA-Natural have replaced bronze, brass, steel, and aluminum in various mechanical applications.Data provided by the manufacturer, Cast Nylons Limited.The dat.. |
|||
Shear Strength | 72.0 MPa | 10400 psi | ASTM D732 |
Cast Nylons Nycast® 6PA-MoS2 Nylon 6 NYCAST® 6PA-MoS2 is a molybdenum disulphide filled Type 6 cast nylon. Finely divided MoS2 particles are suspended in the melt during polymerization. This gives the NYCAST® 6PA-MoS2 products improv.. |
|||
Shear Strength | 72.0 MPa | 10400 psi | ASTM D732 |
Cast Nylons Nycast® 6PA-Natural Nylon 6, Food Grade NYCAST® 6 PA-Natural along with NYCAST® 6 PA-Blue are two of the most widely used cast nylons in industry. Nylons have replaced bronze, brass, steel, and aluminum in various mechanical applicatio.. |
|||
Shear Strength | 72.0 MPa | 10400 psi | ASTM D732 |
Cast Nylons Nycast® XHA Heat Stabilized Nylon 6 Heat stabilized Cast Nylon 6 adds up to 20 degrees F higher continuous operation temperature for those applications that require additional temperature resistance beyond the standard resistance. Dat.. |
|||
Shear Strength | 72.0 MPa | 10400 psi | ASTM D732 |
PolyOne Edgetek® NI-30GF/000 Nylon 6/10 - 30% Glass Fiber Reinforced
(discontinued **) Data provided by PolyOne. |