Secant Modulus, TD 0.220 GPa
31.9 ksi
at 1%; ASTM D882
NOVA Chemicals Novapol® 5% LF-0718-A in PF-0118-B LDPE Film Resin
Improves gloss and reduces haze in blends with LLDPE, Improves melt strength and increases output in blends with LLDPEApplications: Blends with LLDPEAdditives: Base resinFilm properties are typical ..
Secant Modulus, TD 0.220 GPa
31.9 ksi
ASTM D882
Chevron Phillips 6335 LLDPE Cast/Blown Film Resin, Butene Copolymer  (discontinued **)
Resin Type: Butene CopolymerCharacteristics: Good Optics, Good Drawdown, Can be used straight or blended with LDPE or HDPE, Can be used in blown or cast applicationsApplications:Bakery Films, Coextr..
Secant Modulus, TD 0.220 GPa
31.9 ksi
ASTM D882
Chevron Phillips 7120T LLDPE Cast/Blown Resin, Hexene Copolymer  (discontinued **)
Resin Type: Hexene CopolymerCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPEApplications:Stretch Wrap, CoextrusionsProcessing Conditio..
Secant Modulus, TD 0.220 GPa
31.9 ksi
ASTM D882
NOVA Chemicals Sclair® 11D1 Butene LLDPE Film Resin  (discontinued **)
Film Properties. Features: Strength and toughness, good sealing properties, suitable for narrow die gaps.Applications: Industrial packaging, heavy duty sacks.Data provided by the manufacturer.
Secant Modulus, TD 0.220 GPa
31.9 ksi
ASTM D882
Chevron Phillips 5554-D LDPE High Clarity, Medium Impact, Low Slip Film Resin  (discontinued **)
Resin Type: HomopolymerCharacteristics: Excellent Clarity, Good Impact Strength, Good Sealability, Low SlipApplications:Food Packaging, Case Shrink Wrap, LaminationsProcessing Conditions: Extruder 6..
Secant Modulus, TD 0.220 GPa
31.9 ksi
ASTM D882
Chevron Phillips 5758 LDPE High Clarity, High Impact Film Resin  (discontinued **)
Resin Type: HomopolymerCharacteristics: High Clarity, Excellent Impact Strength, Medium Slip, Medium Antiblock, Moderately High Coefficient of Friction, Easy Openability of BagsApplications:Case Shr..
Secant Modulus, TD 0.220 GPa
31.9 ksi
0.01; ASTM D882
Eastman 1925F Polyethylene Film  (discontinued **)
Polyethylene 1925F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require heat-sealing treated-to-treated film surfaces and where good..
Secant Modulus, TD 0.220 GPa
31.9 ksi
1% Secant; ASTM D882
Eastman E6838-795F Polyethylene  (discontinued **)
E6838-795F is a low density formulation with no slip or antiblock level. It is suggested for film applications that require a good balance of properties such as converter film for industrial packag..
Secant Modulus, TD 0.220 GPa
31.9 ksi
1% Secant; ASTM D882
Eastman E6838-796F Polyethylene  (discontinued **)
E6838-796F is a low density formulation with no slip or antiblock. It is suggested for film applications requiring a good balance of properties, such as converter film for industrial packaging, gen..
Secant Modulus, TD 0.220 GPa
31.9 ksi
ASTM D882
ExxonMobil Escorene® LD-103 LDPE Industrial Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer industrial film resin with excellent toughness. LD-103 has a low melt index which gives excellent impact strength and melt strength o..
Secant Modulus, TD 0.220 GPa
31.9 ksi
ASTM D882
Huntsman PE5030 Extrusion Coating Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Good draw down, low neck-in, good heat sealability and adhesion, low smoking, and excellent printabilityApplications: Extrusion: coating grade and general coa..
Secant Modulus, TD 0.220 GPa
31.9 ksi
ASTM D882
Huntsman PE5032 Extrusion Coating Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Excellent draw down, low neck-in, excellent heat sealability, good adhesion, low smoking, no edge weave, and excellent printability.Applications: Extrusion: c..
Secant Modulus, TD 0.220 GPa
31.9 ksi
ASTM D882
ExxonMobil Escorene® LD-334 EVA Film Resin, Clarity, High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 4.2% vinyl acetate copolymer, clarity film resin. The low melt index and comonomer context of this resin help produce films with superior impact ..
Secant Modulus, TD 0.220 GPa
31.9 ksi
ASTM D882-A
Borealis Himod™ FT6273 LDPE for Film
Himod FT6273 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i..
Secant Modulus, TD 0.220 GPa
31.9 ksi
ASTM D882-A
Borealis Himod™ FT6274 LDPE for Film
Himod FT6274 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i..
Secant Modulus, TD 0.220 GPa
31.9 ksi
ASTM D882
Chevron Phillips 5754 LDPE High Clarity, High Impact Film Resin for General Purpose Packaging
Resin Type: HomopolymerCharacteristics: Excellent Impact Strength, High Clarity, Medium Slip, Medium Antiblock, Low Coefficient of Friction, Good OpenabilityApplications:Heavy Produce Bags, Frozen F..
Secant Modulus, TD 0.220 GPa
31.9 ksi
ASTM D882
Chevron Phillips MarFlex® 5755 LDPE High Clarity, High Impact Film Resin
Resin Type: HomopolymerCharacteristics: High Clarity, Excellent Impact Strength, Medium Slip, High Antiblock, Moderately High Coefficient of Friction, Excellent ProcessabilityApplications:Case Shrin..
Secant Modulus, TD 0.220 GPa
31.9 ksi
ASTM D882
Chevron Phillips 6335B LLDPE Cast/Blown Film Resin, Butene Copolymer  (discontinued **)
Resin Type: Butene Copolymer, Medium Slip Version of 6335Characteristics: Good Optics, Good Drawdown, Can be used straight or blended with LDPE or HDPE, Can be used in blown or cast applications, Lo..
Secant Modulus, TD 0.220 GPa
31.9 ksi
ASTM D882
NOVA Chemicals Sclair® 11M1 Butene LLDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, strength and toughness.Applications: Co-extrusion.Data provided by the manufacturer.
Secant Modulus, TD 0.220 GPa
31.9 ksi
1% Secant; ASTM D882
Eastman D4036-F Polyethylene  (discontinued **)
D4036-F is a low density formulation with high slip and high antiblock. It is suggested for film applications requiring a good balance of properties, such as converter film for industrial and gener..
Secant Modulus, TD 0.220 GPa
31.9 ksi
1% Secant; ASTM D882
Eastman E6838-963F Polyethylene  (discontinued **)
E6838-963F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require a good balance of physical and optical properties.List of Applicati..