Polymer Property : Heat Seal Strength Initiation Temperature = 392 °F Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Heat Seal Strength Initiation Temperature 120 - 200 °C
248 - 392 °F
DuPont Teijin Films Melinex® CORE 2 Polyester Film
Melinex® CORE 2 is a two-side heat sealable, opaque white polyester film which is ideal in specialty card laminate applications. This film can be heat sealed to itself and other polyesters, as well..