Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Creep Modulus, 1000 hours = 232000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1000 hours 1600 MPa

@Temperature 23.0 °C
232000 psi

@Temperature 73.4 °F
ISO 899
DuPont Performance Polymers Delrin® 500AL NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 500AL is a medium viscosity acetal homopolymer, with an advanced system of lubrication for applications requiring low wear and/or coefficient of friction against steel, itself or other plas..
Tensile Creep Modulus, 1000 hours 1600 MPa

@Temperature 23.0 °C
232000 psi

@Temperature 73.4 °F
ISO 899
DuPont Performance Polymers Delrin® FG500AL NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® FG500AL is a medium viscosity acetal homopolymer, lubricated for low wear and /or coefficient of friction. It has been developed for consideration into applications such as parts for the fo..
Tensile Creep Modulus, 1000 hours 1600 MPa

@Temperature 23.0 °C
232000 psi

@Temperature 73.4 °F
ISO 899
DuPont Performance Polymers Delrin® FG500P NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® FG500P is a medium viscosity acetal homopolymer, with improved thermal stability. It has been developed for consideration into applications such as parts for the food industry.Information p..
Tensile Creep Modulus, 1000 hours 1600 MPa
232000 psi
Covestro Bayblend® T 65 MN Polycarbonate/ABS Blend
High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy.Applications: Interior automotive components.Information provided by Bayer.As of 1 September 2015,..
Tensile Creep Modulus, 1000 hours 1600 MPa

@Time 3.60e+6 sec
232000 psi

@Time 1000 hour
ISO 899-1
DuPont Performance Polymers Delrin® 500AL NC010 Acetal (POM)  (Unverified Data**)
Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500AL is a medium viscosity acetal homopolymer with an advanced system of lubrication for applications requiring ..
Tensile Creep Modulus, 1000 hours 1600 MPa

@Temperature 23.0 °C
232000 psi

@Temperature 73.4 °F
ISO 899
DuPont Performance Polymers Delrin® 500PE NC010A Acetal Homopolymer
Delrin® 500PE NC010A is a medium viscosity acetal homopolymer, an enhanced version of Delrin® 500P with extremely low VOC emissions. It has improved processing thermal stability, and good mechanic..
Tensile Creep Modulus, 1000 hours 1600 MPa

@Time 3.60e+6 sec
232000 psi

@Time 1000 hour
ISO 899-1
DuPont Performance Polymers Delrin® FG500AL NC010 Acetal (POM)  (Unverified Data**)
Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications Delrin FG500AL is a medium viscosity acetal homopolymer lubricated for low wear ..
Tensile Creep Modulus, 1000 hours 1600 MPa

@Time 3.60e+6 sec
232000 psi

@Time 1000 hour
ISO 899-1
DuPont Performance Polymers Delrin® 500P NC010 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer with Improved Processing Delrin 500P is a medium viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical ..
Tensile Creep Modulus, 1000 hours 1600 MPa
232000 psi
BASF Polystyrol® 445 E WU Impact Grade Polystyrene (Europe)
Easy flowing, heat-resistant, medium-impact, flame-retardant grade. Application example: electrical distribution boxes.Data was collected by ISO methods and provided by BASF.
Tensile Creep Modulus, 1000 hours 1600 MPa
232000 psi
BASF Polystyrol® 585 K Impact Grade Polystyrene (Europe)
Special high gloss, high-impact grade for all types of housings. Basis product for gloss capping.Data was collected by ISO methods and provided by BASF.
Tensile Creep Modulus, 1000 hours 1600 MPa
232000 psi
Arkema Group Oroglas® VM Acrylic, Injection Molding Grade  (discontinued **)
OROGLAS VM is an injection molding grade with a medium heat resistance and easy flow.OROGLAS VM is particularly suitable to improve mold filling of technical parts.The VM L version has been speciall..
Tensile Creep Modulus, 1000 hours 1600 MPa

@Strain <=0.500 %
232000 psi

@Strain <=0.500 %
ISO 899-1
Styrolution Luran® S KR 2861/1 C Colored ASA+PC
Description: Grade with high heat resistance for injection molding and extrusion.Applications: Interior and exterior automotive parts, and electrical housings.Information provided by STYROLUTION, wh..
Tensile Creep Modulus, 1000 hours 1600 MPa
232000 psi
ISO 899-1
Lanxess Pocan® S 7020 000000 PBT
PBT, non-reinforced, injection molding, extrusion, flame retardant, impact modified