Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1000 hours | 3500 MPa | 508000 psi | ISO 899-1 |
Lanxess Durethan® BKV 25 H2.0 LT 904040 Nylon 6, 25% Glass Fiber PA 6, injection molding grade, 25% glass fibers, good heat-ageing resistance, laser-weldable |
|||
Tensile Creep Modulus, 1000 hours | 3500 MPa @Time 3.60e+6 sec |
508000 psi @Time 1000 hour |
ISO 899-1 |
DuPont Performance Polymers Delrin® 510GR NC000 Acetal (POM)
(Unverified Data**) 10% Glass Reinforced Medium Viscosity Acetal Homopolymer Delrin 510GR is a 10% glass reinforced acetal homopolymer for injection molding. It has high strength stiffness and high deflection temperatu.. |
|||
Tensile Creep Modulus, 1000 hours | 3500 MPa @Time 3.60e+6 sec |
508000 psi @Time 1000 hour |
ISO 899-1 |
DuPont Performance Polymers Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT) 10% Glass Reinforced Flame Retardant Polybutylene Terephthalate Information provided by DuPont Performance Polymers |