Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1000 hours 3500 MPa
508000 psi
ISO 899-1
Lanxess Durethan® BKV 25 H2.0 LT 904040 Nylon 6, 25% Glass Fiber
PA 6, injection molding grade, 25% glass fibers, good heat-ageing resistance, laser-weldable
Tensile Creep Modulus, 1000 hours 3500 MPa

@Time 3.60e+6 sec
508000 psi

@Time 1000 hour
ISO 899-1
DuPont Performance Polymers Delrin® 510GR NC000 Acetal (POM)  (Unverified Data**)
10% Glass Reinforced Medium Viscosity Acetal Homopolymer Delrin 510GR is a 10% glass reinforced acetal homopolymer for injection molding. It has high strength stiffness and high deflection temperatu..
Tensile Creep Modulus, 1000 hours 3500 MPa

@Time 3.60e+6 sec
508000 psi

@Time 1000 hour
ISO 899-1
DuPont Performance Polymers Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT)
10% Glass Reinforced Flame Retardant Polybutylene Terephthalate Information provided by DuPont Performance Polymers