Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1000 hours 2000 - 5000 MPa
290000 - 725000 psi
Average value: 3580 MPa Grade Count:6
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% ..