Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1000 hours 400 - 1450 MPa
58000 - 210000 psi
Average value: 1160 MPa Grade Count:40
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
Tensile Creep Modulus, 1000 hours 400 - 840 MPa
58000 - 122000 psi
Average value: 663 MPa Grade Count:3
Overview of materials for Nylon 66, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr..
Tensile Creep Modulus, 1000 hours 400 MPa
58000 psi
LyondellBasell Lupolen® 6031 M HDPE, Injection Molding Grade
Easy flow, injection molding grade for fruit crates, tote boxes and bottle crates, cartridges, protective headgear, buckets, dishes, cartridges for adhesive film canisters, aerosol lids, child seats..
Tensile Creep Modulus, 1000 hours 400 MPa
58000 psi
At 1% Deformation; DIN 53444
Wolf Kunststoff ZEDEX® ZX-100EL55 A1F Polymer Alloy, Elastomer Modified
Main Characteristics: Rubbery; Soft; High shock absorption; High impact resistance; Elongation > 300%Applications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automitve Technol..
Tensile Creep Modulus, 1000 hours 400 MPa
58000 psi
23°C; ISO 899; DIN 53444
Zell-Metall Engineering Plastics Zellamid 250 (PA6.6) at 50% RH
Zellamid® 250 is noted for its high temperature resistance and high tensile strength. It is the hardest and most rigid type of extruded Nylon. Main characteristics are high resistance to fuels, oil..
Tensile Creep Modulus, 1000 hours 400 MPa
58000 psi
ISO 899-1
BASF Ultraform® N2650 Z6 (LEV) POM
Description: Is a POM + PUR, elastomer-modified injection-molding grade for applications requiring the highest impact strength together with low stiffness.Information provided by BASF
Tensile Creep Modulus, 1000 hours 400 - 1050 MPa
58000 - 152000 psi
Average value: 845 MPa Grade Count:16
Overview of materials for Acetal Copolymer, Impact Modified