Mechanical Properties | Metric | English | Comments |
---|---|---|---|
50% Modulus | 0.00190 GPa | 0.276 ksi | ISO 527-2/5A/500 |
Lubrizol Advanced Materials PEARLTHANE® 11T65D Thermoplastic Polyurethane Elastomer Type : Pearlthane® 11T65D is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining very high hardness with excellent me.. |
|||
50% Modulus | 0.00190 GPa | 0.276 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 5565 ASTM D3568 FormulationNordel® IP 5565 |
|||
50% Modulus | 0.00190 GPa | 0.276 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 5565 General Purpose Molding FormulationNordel® IP 5565 |
|||
50% Modulus | 0.00190 GPa | 0.276 ksi | Vulcanizate, Press cured, TC95 +3min at 180°C |
Dow Nordel® IP 4570 Heat Resistant Peroxide Compound FormulationNordel® IP 4570 |
|||
50% Modulus | 0.00190 GPa | 0.276 ksi | ASTM D412 |
C.O.I.M. LARIPUR® LPR6518 Plasticized Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |