Mechanical Properties Metric English Comments
50% Modulus 0.00190 GPa
0.276 ksi
ISO 527-2/5A/500
Lubrizol Advanced Materials PEARLTHANE® 11T65D Thermoplastic Polyurethane Elastomer
Type : Pearlthane® 11T65D is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining very high hardness with excellent me..
50% Modulus 0.00190 GPa
0.276 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 5565 ASTM D3568
FormulationNordel® IP 5565
50% Modulus 0.00190 GPa
0.276 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 5565 General Purpose Molding
FormulationNordel® IP 5565
50% Modulus 0.00190 GPa
0.276 ksi
Vulcanizate, Press cured, TC95 +3min at 180°C
Dow Nordel® IP 4570 Heat Resistant Peroxide Compound
FormulationNordel® IP 4570
50% Modulus 0.00190 GPa
0.276 ksi
ASTM D412
C.O.I.M. LARIPUR® LPR6518 Plasticized Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..