Mechanical Properties Metric English Comments
Gardner Impact 36.0 J

@Temperature 23.0 °C
26.6 ft-lb

@Temperature 73.4 °F
ASTM D5420
Flint Hills AP7810-HS Polypropylene Ultra High Impact Copolymer
Features: Excellent stiffness and low temperature ductility.Applications: Injection Molding: Automotive interior energy management solutionsInformation Provided by Flint Hills Resources
Gardner Impact 36.0 J

@Temperature -30.0 °C
26.6 ft-lb

@Temperature -22.0 °F
ASTM D5420
Flint Hills AP7810-HS Polypropylene Ultra High Impact Copolymer
Features: Excellent stiffness and low temperature ductility.Applications: Injection Molding: Automotive interior energy management solutionsInformation Provided by Flint Hills Resources