Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 36.0 J @Temperature 23.0 °C |
26.6 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Flint Hills AP7810-HS Polypropylene Ultra High Impact Copolymer Features: Excellent stiffness and low temperature ductility.Applications: Injection Molding: Automotive interior energy management solutionsInformation Provided by Flint Hills Resources |
|||
Gardner Impact | 36.0 J @Temperature -30.0 °C |
26.6 ft-lb @Temperature -22.0 °F |
ASTM D5420 |
Flint Hills AP7810-HS Polypropylene Ultra High Impact Copolymer Features: Excellent stiffness and low temperature ductility.Applications: Injection Molding: Automotive interior energy management solutionsInformation Provided by Flint Hills Resources |