Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 11.0 GPa @Temperature -40.0 °C |
1600 ksi @Temperature -40.0 °F |
ISO 178 |
DuPont Performance Polymers Rynite® FR530 BK507 PET
(Unverified Data**) Rynite® FR530 BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 11.0 GPa @Thickness 1.57 mm |
1600 ksi @Thickness 0.0620 in |
LW |
Industrial Laminates/Norplex NP841 Glass Fabric
(discontinued **) Description: Woven glass fabric with phenolic resin. Contains Kocite® for controlled conductivity. Acts as static electricity drain to protect electrical and electronic equipment.Thickness Tested: .. |
|||
Flexural Modulus | 11.0 GPa @Temperature 23.0 °C |
1600 ksi @Temperature 73.4 °F |
DAM; ASTM D790 |
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612
(Unverified Data**) Zytel® 77G43L BK031 is a 43% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 11.0 GPa @Temperature 23.0 °C |
1600 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612
(Unverified Data**) Zytel® 77G43L BK031 is a 43% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 11.0 GPa @Temperature 23.0 °C |
1600 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612
(Unverified Data**) Zytel® 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 11.0 GPa @Temperature 23.0 °C |
1600 ksi @Temperature 73.4 °F |
DAM; ASTM D790 |
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612