Mechanical Properties Metric English Comments
Flexural Modulus 11.0 GPa

@Temperature -40.0 °C
1600 ksi

@Temperature -40.0 °F
ISO 178
DuPont Performance Polymers Rynite® FR530 BK507 PET  (Unverified Data**)
Rynite® FR530 BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers
Flexural Modulus 11.0 GPa

@Thickness 1.57 mm
1600 ksi

@Thickness 0.0620 in
LW
Industrial Laminates/Norplex NP841 Glass Fabric  (discontinued **)
Description: Woven glass fabric with phenolic resin. Contains Kocite® for controlled conductivity. Acts as static electricity drain to protect electrical and electronic equipment.Thickness Tested: ..
Flexural Modulus 11.0 GPa

@Temperature 23.0 °C
1600 ksi

@Temperature 73.4 °F
DAM; ASTM D790
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612  (Unverified Data**)
Zytel® 77G43L BK031 is a 43% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
Flexural Modulus 11.0 GPa

@Temperature 23.0 °C
1600 ksi

@Temperature 73.4 °F
DAM; ISO 178
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612  (Unverified Data**)
Zytel® 77G43L BK031 is a 43% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
Flexural Modulus 11.0 GPa

@Temperature 23.0 °C
1600 ksi

@Temperature 73.4 °F
DAM; ISO 178
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612  (Unverified Data**)
Zytel® 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
Flexural Modulus 11.0 GPa

@Temperature 23.0 °C
1600 ksi

@Temperature 73.4 °F
DAM; ASTM D790
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612  (Unverified Data**)
Zytel® 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers