Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.70 GPa @Temperature 23.0 °C |
247 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6
(Unverified Data**) Zytel® ST7301 NC010 is a Super Tough, heat stabilized, lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide temperature and humidity.. |
|||
Flexural Modulus | 1.70 GPa @Temperature 130 °C |
247 ksi @Temperature 266 °F |
|
Hybrid Plastics CO6U50.01 Nanoreinforced® Cyclic Olefin Copolymer Impact modified, UV stabilizedThe exceptional heat distortion temperature and low density of cyclic olefin copolymers (COC) makes them excellent materials for high temperature applications where low.. |
|||
Flexural Modulus | 1.70 GPa @Temperature 130 °C |
247 ksi @Temperature 266 °F |
|
Hybrid Plastics CO6U50.02 Nanoreinforced® Cyclic Olefin Copolymer Impact modified, flame retardantThe exceptional heat distortion temperature and low density of cyclic olefin copolymers (COC) makes them excellent materials for high temperature applications where l.. |
|||
Flexural Modulus | 1.70 GPa @Temperature 260 °C |
247 ksi @Temperature 500 °F |
ASTM D790 |
Saint-Gobain Meldin® 7001 CM Compression Molded Polyimide Meldin® 7001 CM unfilled polyimide base resin, compression moldedSpecification Qualifications:Satisfies Type I P for ASTM D 6456-99: Standard Specification for Finished Parts Made from Polyimide .. |
|||
Flexural Modulus | 1.70 GPa @Temperature 80.0 °C |
247 ksi @Temperature 176 °F |
Practical Use (Water Absorption 3.0%); ASTM-D790 |
Toyobo GLAMIDE® T-400G15 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 1.70 GPa @Temperature 80.0 °C |
247 ksi @Temperature 176 °F |
Practical Use (Water Absorption 2.3%); ASTM-D790 |
Toyobo GLAMIDE® T-422-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 1.70 GPa @Temperature 80.0 °C |
247 ksi @Temperature 176 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-777-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 1.70 GPa @Temperature 150 °C |
247 ksi @Temperature 302 °F |
ISO 178 |
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT
(Unverified Data**) Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |