Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.30 GPa @Temperature -20.0 °C |
334 ksi @Temperature -4.00 °F |
ISO 178 |
Polykemi AB POLYfill PPHC K3020 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 2.30 GPa @Temperature 23.0 °C |
334 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® 157HSL BK010 Nylon 612
(Unverified Data**) Zytel® 157HSL BK010 is a heat stabilized, weatherable, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 2.30 GPa @Temperature 23.0 °C |
334 ksi @Temperature 73.4 °F |
Practical Use (Water Absorption 2.1%); ASTM-D790 |
Toyobo GLAMIDE® NB-5620S Nylon/Olefin GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 2.30 GPa @Temperature 80.0 °C |
334 ksi @Temperature 176 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-400G15 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 2.30 GPa @Temperature -40.0 °C |
334 ksi @Temperature -40.0 °F |
Practical Use (Water Absorption 2.9%); ASTM-D790 |
Toyobo GLAMIDE® TY-102ND Nylon/Elastomer GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 2.30 GPa @Temperature 163 °C |
334 ksi @Temperature 325 °F |
|
Hexcel® HexPly® 954-3 Curing Cyanate Resin HexPly® 954-3 is a 350°F (177°C) curing cyanate resin with excellent resistance to moisture absorption, outgassing and microcracking. HexPly® 954-3 is formulated for autoclave or press molding u.. |
|||
Flexural Modulus | 2.30 GPa @Temperature 163 °C |
334 ksi @Temperature 325 °F |
Wet (Immersion at 170°F for 7 days) |
Hexcel® HexPly® 954-2A Curing Cyanate Resin HexPly® 954-2A is a 350°F (177°C) curing toughened cyanate resin with low moisture absorption, and excellent microcracking resistance. HexPly® 954-2A is formulated for autoclave or press molding.. |
|||
Flexural Modulus | 2.30 GPa @Temperature 250 °C |
334 ksi @Temperature 482 °F |
EN ISO 178 |
Ensinger TECASINT™ 2011 Polyimide (PI) TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications... |
|||
Flexural Modulus | 2.30 GPa @Temperature 23.0 °C |
334 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® 7301 NC010 Nylon 6
(Unverified Data**) Zytel® 7301 NC010 is a general purpose, unlubricated polyamide 6 resin for extrusion applications.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 2.30 GPa @Temperature -20.0 °C |
334 ksi @Temperature -4.00 °F |
ISO 178 |
Polykemi AB POLYfill PPHC K5020 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 2.30 GPa @Temperature -20.0 °C |
334 ksi @Temperature -4.00 °F |
ISO 178 |
Polykemi AB POLYfill PPHC K8020 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 2.30 GPa @Temperature -20.0 °C |
334 ksi @Temperature -4.00 °F |
ISO 178 |
Polykemi AB POLYfill PPHC K9020 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |