Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 4.27 J/cm @Thickness 12.7 mm |
8.00 ft-lb/in @Thickness 0.500 in |
CW, E-48/50 |
Industrial Laminates/Norplex NP180 Synthetic Fabric
(discontinued **) Description: aramid fabric material with a high performance epoxy resin matrix. Excellent electrical and mechanical properties at elevated temperatures and in adverse environments.Thickness Tested: .. |
|||
Izod Impact, Unnotched | 4.27 J/cm @Thickness 12.7 mm |
8.00 ft-lb/in @Thickness 0.500 in |
CW, E-48/50 |
Industrial Laminates/Norplex NP841 Glass Fabric
(discontinued **) Description: Woven glass fabric with phenolic resin. Contains Kocite® for controlled conductivity. Acts as static electricity drain to protect electrical and electronic equipment.Thickness Tested: .. |
|||
Izod Impact, Unnotched | 4.27 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
8.00 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Lubrizol Isoplast® 101LGF40NAT Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Izod Impact, Unnotched | 4.27 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
8.00 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256 |
Lubrizol Isoplast® 101LGF40NAT Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |