Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.03 GPa | 440 ksi | Tangent; ASTM D790 |
RheTech Products FRP257-00 32% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Natural Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D638 |
Network Polymers MS 300 Styrene Methyl Methacrylate Copolymer Description: Styrene Methyl Methacrylate CopolymerInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000HL Nylon 6/6 Available in North America Additive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and Lubricated RoHS Compliant Auto Specifications: FORD WSK-M4D648-A Color: Black Form: Pellets Processi.. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Polymer Resources NY66-GP2 General Purpose Nylon 66, Nucleated General Purpose Nylon 66, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry.. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000EHL Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000L2 Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000MDL Nylon 6/6
(discontinued **) Available in North America Additive: Molybdenum Disulfide Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedForm: Pellets Information provided by Ravago. |
|||
Flexural Modulus | 3.03 - 14.8 GPa | 440 - 2150 ksi | Average value: 7.75 GPa Grade Count:104 |
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Flexural Modulus | 3.03 - 5.52 GPa | 440 - 800 ksi | Average value: 4.39 GPa Grade Count:10 |
Overview of materials for Nylon 11 with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are includ.. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | 2.0 in/min; ASTM D790 |
LTL Color Compounds ColorFast® PEI1000 Polyetherimide Injection and extrusion grade polyetherimide, high temperatureAll information provided by LTL Color Compounders, Inc. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Global TPP-130 30% Talc Filled Polypropylene Information provided by Global Polymers Corporation. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | Method I (3 point load), Procedure B); ASTM D790 |
Multibase Multi-Flamâ„¢ 2012 HFR 24 Polypropylene Features:Flame Retardant Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Techmer ES Electrablend® PC/ABS 033009 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: Electrically Conductive and ESD ProtectionInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Techmer ES Electrablend® POM Acetal Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveTPCI# 9961114Information provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Techmer ES HiFill® PA6 AF Colors Availability: North AmericaForms: PelletsFiller/Reinforcement: Aramid FiberAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricateAppearance: Colors AvailableInformation provi.. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Techmer ES HiFill® POM CO 0150 S Acetal Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalFeatures: CopolymerInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Techmer ES HiFill® POM CO 0167 S1 LE Acetal Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalFeatures: Copolymer and Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Techmer ES Plastiblend® PC/ABS 8800 Availability: North AmericaForms: PelletsFeatures: High Impact Resistance and High Temperature StrengthProcessing Method: Profile ExtrusionInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Techmer ES HiFill® PPSU A1 0200 B LE Availability: North AmericaForms: PelletsFeatures: High Density and Low ExtractablesAppearance: OpaqueInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Ensinger Tecamid® 6/6 Nylon (PA66) Type 6/6 is a general purpose standard grade nylon. Extruded in natural and black. (Weather Resistant Black Grade is also available.)Information provided by Ensinger, Inc. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Ensinger Tecamid® HS Nylon (PA) Heat Stabilized nylon, increased ability to withstand the negative effects of heat exposure and increased overall service temperature over nylon 6/6.Information provided by Ensinger, Inc. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Ensinger Tecatron® XP-76 Compression Molded PPS Compound, 55% PTFE Filled Seal Material Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D-790 |
Axiall 6316 Rigid PVC, Molding Georgia Gulf 6316 is an economical high flow rigid PVC fittings compound designed for drain, waste and vent applications, where higher impact properties are desired. This compound is characterized .. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | |
Abatron AboCast 8504-5 One-Component Epoxy AboCast 8504-5 is a clear, plasticized one-component epoxy system with very high strength and impact. It provides exceptional physical properties and thermal shock resistance from sub-zero to modera.. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D-790 |
Axiall 7020 Rigid PVC, Extrusion Georgia Gulf 7020 is a special purpose rigid PVC profile extrusion compound designed for thin-wall applications requiring the following properties: Impact Strength & ToughnessDimensional StabilityF.. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Asahi Kasei Thermylene® P6-20FM-2601 20% Glass/Mineral, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | secant; ASTM D790 |
Spartech PP5340 Mica Reinforced Homopolymer Information provided by Spartech |