Material Notes:
Information provided by Global Polymers Corporation.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
L; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.7 MPa
4600 psi
ASTM D638
Flexural Modulus 3.03 GPa
440 ksi
ASTM D790
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 124 °C
255 °F
ASTM D648