Mechanical Properties Metric English Comments
Flexural Modulus 6.89 - 21.4 GPa
1000 - 3100 ksi
Average value: 12.0 GPa Grade Count:20
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu..
Flexural Modulus 6.21 - 21.4 GPa
900 - 3100 ksi
Average value: 13.4 GPa Grade Count:4
Overview of materials for Acrylic/Polycarbonate Alloy, Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Carbon Fiber Filler". Each property range of values reported is minimum and..