Polymer Property : Flexural Modulus = 0.138 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.138 - 1.77 GPa
20.0 - 257 ksi
Average value: 0.736 GPa Grade Count:10
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Blow Molding Grade". Each property range of values reported is m..
Flexural Modulus 0.138 GPa
20.0 ksi
2% Secant, 12.7 mm/min; ASTM D790
Eastman D4056-P Polyethylene  (discontinued **)
Polyethylene D4056-P is a natural low density material with an 80 melt index.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no lon..
Flexural Modulus 0.138 GPa
20.0 ksi
ASTM D790
Multibase Multi-Flex® D 4201 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Heat StabilizedOzone Resistant General Purpose Forms:PelletsProcessing Method:Injection MoldingBlow MoldingExtrusion Uses: Automotive ApplicationsInformation p..
Flexural Modulus 0.138 GPa
20.0 ksi
ASTM D790
Multibase Multi-Flex® G 7827 Black TPE Styrene Ethylene Butylene Styrene Block Copolymer
Forms: PelletsProcessing Methods:Injection Molding Uses: Automotive ApplicationsInformation provided by Multibase
Flexural Modulus 0.138 GPa
20.0 ksi
ASTM D790
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains ..
Flexural Modulus 0.138 GPa
20.0 ksi
ASTM D790
Teknor Apex TEKRON® 4300-D88A Thermoplastic Elastomer
Information provided by Teknor Apex Company
Flexural Modulus 0.138 GPa
20.0 ksi
ASTM D790
Teknor Apex TEKRON® 4300LM-P88-1 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Flexural Modulus 0.138 GPa
20.0 ksi
ASTM D790
Teknor Apex Telcar® TL EF-6100 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Flexural Modulus 0.138 GPa
20.0 ksi
ASTM D790
DuPont Keldax® 6868 Filled Thermoplastic Ethylene Polymer
A low fog filled thermoplastic ethylene polymer that provides acoustical sound barrier performance in automotive, construction, and industrial applications.Processing Method: ExtrusionSheetAvailabil..
Flexural Modulus 0.138 GPa
20.0 ksi
ASTM D790
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains ..
Flexural Modulus 0.138 GPa
20.0 ksi
ASTM D790
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains ..
Flexural Modulus 0.138 GPa
20.0 ksi
ASTM D790
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains ..
Flexural Modulus 0.138 GPa
20.0 ksi
ASTM D790
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains ..
Flexural Modulus 0.138 GPa
20.0 ksi
ASTM D790
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains ..