Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Amco PRIMATOP LDPE 023919 Blow Molding Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Blow Molding Grade
Manufacturer Amco Plastic Materials
Trade Name PRIMATOP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Amco PRIMATOP LDPE 023919 Blow Molding Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LDPE 023919 features good heat sealing latitude and easy processability. Applications include food contact, squeeze bottles, and non-escr.Former A-Top Polymers product; part of Amco product line since 2013.
Physical Properties Metric English Comments
Density 0.919 g/cc
0.0332 lb/in³
ASTM D1505
ESCR 100% Igepal® 100 hour
100 hour
Condition B, F50; ASTM D1693
Melt Index of Compound 2.3 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.3 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 8.48 MPa
1230 psi
50 mm/min; ASTM D638
Elongation at Break >= 630 %
>= 630 %
50 mm/min; ASTM D638
Flexural Modulus 0.214 GPa
31.0 ksi
ASTM D790