Mechanical Properties Metric English Comments
Flexural Modulus 0.450 GPa

@Temperature 23.0 °C
65.3 ksi

@Temperature 73.4 °F
ISO 178
Polykemi AB POLYelast TPE EC88R Thermoplastic Elastomer, PP/EPDM
Information provided by Polykemi AB
Flexural Modulus 0.450 GPa

@Temperature 23.0 °C
65.3 ksi

@Temperature 73.4 °F
ISO 178
Polykemi AB POLYelast TPE ED80 D40 UV Thermoplastic Elastomer
Information provided by Polykemi AB
Flexural Modulus 0.450 GPa

@Temperature 120 °C
65.3 ksi

@Temperature 248 °F
ASTM D790
LATI LATILUB 73/13-20T Polyoxymethylene Base (POM), 10% Mixed PTFE Self Lubricating Plastic  (Unverified D
Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri..
Flexural Modulus 0.450 GPa
65.3 ksi
ISO 178
Borealis Borsoft™ SD200CF High Impact Polypropylene Random Heterophasic Copolymer for Cast Film
Borsoft SD200CF is a very soft random heterophasic copolymer, suitable for use on chill roll process. The product combines unique softness with outstanding mechanical properties making it the ideal..
Flexural Modulus 0.450 GPa
65.3 ksi
ASTM-D790
Polyram PlusTek RD101 Nylon 12, Injection Molding
Outstanding flexibility polyamide 12 for injection molding applications.Information provided by Polyram Ram On Ind.
Flexural Modulus 0.450 GPa
65.3 ksi
ASTM-D790
Polyram PlusTek PD100 Nylon 12, Injection Molding
Outstanding polyamide 12 for injection molding applications.Information provided by Polyram Ram On Ind.
Flexural Modulus 0.450 GPa
65.3 ksi
SAE J949
Azdel SuperLite® SL551800-100 PP Resin Matrix / 55% Glass Fiber (8 mm Molded Thickness)
AZDEL SuperLite® SL551800-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Flexural Modulus 0.450 - 1.40 GPa

@Temperature 60.0 - 120 °C
65.3 - 203 ksi

@Temperature 140 - 248 °F
Average value: 0.883 GPa Grade Count:1
Overview of materials for Polypropylene with 40% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are..